Corrosion of metals and alloys — Stress corrosion testing — Part 10: Reverse U-bend method
Primary tabs
Reference:
ISO 7539-10:2020
Publication Year:
2020
Domain:
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.